Build to Bond · Balance Bike
Day 4 of 10 · BuildDay 4
Frame Refinement & Bonding Prep
Shape the stays, dry-fit the whole frame, get ready to bond
Welcome the room. Say the day's shape in one sentence.
Recap · whole group
No hands needed · take your time
What do you remember from Day 3?
1What does Dry-fit mean?
2What does Easy fit mean?
3What does Black marks mean?
Say itAnswer out loud. Any answer is a start.
Ask, then count ten before taking an answer. Take offers, never cold call.
How today runs
Run of day
Every step is one of four→Show it→Build it→Say it→Show me
10 minRecap Day 3
95 minStays — refine the fit
Break15 minutes
60 minFull frame dry-assembly + 75 mm
30 minPre-bond quality inspection signed
30 minEpoxy safety briefing + COSHH signed
Read the shape of the day out loud once. Say when the break falls.
For the instructor
Videos today
- 1Wheel alignment & cross-check 02b-wheel-alignment-crosscheck.mp4Today
- 2Jig prep & degreasing the joints 03a-jig-prep-degrease.mp4Watch in order
⚠No internet in the room. Play from the laptop, and open each file before the session to check the sound. Subtitles are on.
Check every file is on the laptop before the session. Subtitles are on.
Non-negotiable · every session
Safety first
- Tool count at start and end — no exceptions
- Glasses + FFP2 dust masks throughout shaping
- Stanley knife: blade away from body; counted in/out (HIGH security); cut-resistant gloves (EN 388 Level D/5) for cutting and filing
- The epoxy safety briefing must be signed before Day 5
Read every rule aloud. Same list as the session risk assessment. Say in full: The epoxy safety briefing must be signed before Day 5; no signed pre-bond inspection = no bonding.
Tomorrow: epoxy
Epoxy: the rules
- Your instructor dispenses the epoxy. You never handle the resin or hardener. The instructor wears chemical-resistant gloves, a face shield and overalls, with ventilation on
- Position the joint within 2–5 minutes, wearing nitrile gloves
- Eyes: eye wash for at least 15 minutes, then medical help — the hardener is corrosive
- Skin: wash with soap and water now; tell your instructor
Read every rule aloud before the COSHH briefing sheet is signed. Same wording as the lesson. Also say: ventilation is on before the epoxy is dispensed; learners wear nitrile gloves (EN 374), safety glasses (EN 166) and long-sleeved cotton overalls; the instructor wears Cat III chemical-resistant nitrile gloves (EN 374), an EN 166 face shield and overalls to dispense.
Show it
Today · you will
What will we do today?
- 1Shape both stays to fit
- 2Cross-check the 75 mm dimension
- 3Dry-fit the whole frame and sign pre-bond QC

One idea per bullet. Say it, then show it.
Say it
Words for today · 1 of 2
Key terms
- Stays
- The two tubes from the seat-tube lug to the dropouts
- 75 mm cross-check
- The dimension both stays must match
- Wheel alignment
- The wheel sits centred between the two stays
Words before content. Same word on the slide, the worksheet and out loud.
Say it
Words for today · 2 of 2
More key words
- Pre-bond QC
- The final quality check before any epoxy
- COSHH
- UK law for safe handling of hazardous substances
- Pot life
- The working time once your instructor has dispensed the epoxy. You position the joint within 2–5 minutes
Second half. Ask for each word back in their own words.
Show it
Day 4 · stays & QC
Shape, cross-check, dry-fit
- Shape both stays; match the 75 mm between lugs
- Over 75 mm? File it back
- Keep the wheel centred; run pre-bond QC; sign COSHH

One idea per bullet. Say it, then show it. Say in full: Over 75 mm? File it back — 2 mm off and the bike won't track straight.
Show it▶Wheel alignment & cross-checkWatch together · the exact clip for today
Play from the laptop if the room has no internet. Ask the slide's question after.
Show it▶Jig prep & degreasing the jointsWatch together · the next stage
Play from the laptop. Pause wherever hands go near the work. The film shows degreasing: on this course we abrade, then wipe with a dry, lint-free cloth. No solvents.
Break
Break · 15 min
Back in the workshop after the count.
Say when the room restarts. Tools down, bench safe, then go.
You do · your evidence
Dry-fit & sign off
- Shape and fit both stays
- Pass the pre-bond QC
- Sign the COSHH entry

Build itYour signed pre-bond inspection and COSHH entry are your evidence.
Offer to scribe at every written task. A scribed verbal answer is valid evidence. Band detail: and your ticket to bond.
Show it▶How to Build a Bamboo Balance Bike: Rear Triangle and DropoutsWatch for: the exact step you are about to do
The lesson page's own build film. No internet in the room — play from the laptop.
Show me
Stop — record evidence
Hand these in
Day 4 evidence
Workbook entry, signed in the room. Signed by you and your tutor.
Verbal answers
Say it and the tutor scribes — that counts.
Goes in your OCN portfolio — LO3, LO4, today.
Hard stop. Signing happens in the room. File before anyone leaves.

Show it
Wrap-up · next
What did we do today?
- Shaped and fitted both stays
- Passed the pre-bond QC
- Signed the epoxy-safety briefing
Next lesson: the irreversible day — epoxy bonding.
Mirror the objectives back. Two words of specific praise per learner.
Show it
Next session · looking ahead
Next lesson: Epoxy Bonding
- Abrade and wipe every joint
- Position the epoxy joint (your instructor dispenses it)
- Seat, align and leave it to cure
Ten seconds. The point is that the next day has a shape.